Specification & sizes

Compare
ComplianceASTM C612
ASTM C612

Mineral Fiber Block and Board Thermal Insulation, Type IVA Compliant

DensityASTM C303

ASTM C303

Actual Density 3.0 lb/ft³ (48 kg/m³)

Dimensional stabilityASTM C356

ASTM C356

Linear Shrinkage <1% @="" 1200°F="">

Dimensions

Please contact ROCKWOOL for sizing information (1-800-265-6878)

 

Thickness

Please contact ROCKWOOL for sizing information (1-800-265-6878)

Reaction to fireASTM E84 (UL 723) - CAN/ULC S102 - CAN/ULC S114 - ASTM E136 - ASTM C411
ASTM E84 (UL 723)

Flame spread index = 0 ; Smoke development index = 0

CAN/ULC S102

Flame spread index = 0 ; Smoke development index = 0

CAN/ULC S114

Behavior of materials at 750°C - Non-Combustible

ASTM E136

Test for Non-Combustibility - Non-Combustible

ASTM C411

Hot Surface Performance - 1200°F

Thermal resistanceASTM C518 (C177)
ASTM C518 (C177) R-value / inch @ 75ºF - 4.1 hr.ft2.F/Btu
 RSI value / 25.4 mm @ 24ºC - 0.72 m2K/W
Acoustical PerformanceASTM C423
Thickness125 Hz250 Hz500 Hz1000 Hz2000 Hz4000 HzNRC
1.5"0.180.440.941.041.021.030.85
2"0.280.61.091.091.051.070.95
3"0.520.961.181.071.051.051.05
4"0.861.111.21.071.081.071.1
Reaction to moistureASTM C1104 - ASTM C1338
ASTM C1104

Moisture Sorption by weight - 0.02%

ASTM C1338

Determination of Fungi Resistance - Passed

Compressive strengthASTM C612
ASTM C165

196psf (9.4 kPa) @ 10% compression

547psf (26.2 kPa) @ 25% compression

Corrosion ResistanceASTM C795 - ASTM C665
ASTM C795

Stress Corrosion Cracking Tendency of Austenitic Stainless Steel - Passed

ASTM C665

Corrosion of Steel - Passed

Back
ASTM C612

Mineral Fiber Block and Board Thermal Insulation, Type IVA Compliant

Back

ASTM C303

Actual Density 3.0 lb/ft³ (48 kg/m³)

Back

ASTM C356

Linear Shrinkage <1% @="" 1200°F="">

Back

Please contact ROCKWOOL for sizing information (1-800-265-6878)

 

Back

Please contact ROCKWOOL for sizing information (1-800-265-6878)

Back
ASTM E84 (UL 723)

Flame spread index = 0 ; Smoke development index = 0

CAN/ULC S102

Flame spread index = 0 ; Smoke development index = 0

CAN/ULC S114

Behavior of materials at 750°C - Non-Combustible

ASTM E136

Test for Non-Combustibility - Non-Combustible

ASTM C411

Hot Surface Performance - 1200°F

Back
ASTM C518 (C177) R-value / inch @ 75ºF - 4.1 hr.ft2.F/Btu
 RSI value / 25.4 mm @ 24ºC - 0.72 m2K/W
Back
Thickness125 Hz250 Hz500 Hz1000 Hz2000 Hz4000 HzNRC
1.5"0.180.440.941.041.021.030.85
2"0.280.61.091.091.051.070.95
3"0.520.961.181.071.051.051.05
4"0.861.111.21.071.081.071.1
Back
ASTM C1104

Moisture Sorption by weight - 0.02%

ASTM C1338

Determination of Fungi Resistance - Passed

Back
ASTM C165

196psf (9.4 kPa) @ 10% compression

547psf (26.2 kPa) @ 25% compression

Back
ASTM C795

Stress Corrosion Cracking Tendency of Austenitic Stainless Steel - Passed

ASTM C665

Corrosion of Steel - Passed

Back

Downloads

documents

 

 

pdf
CoreSolutions-FABROCK-30_Tech Data Sheet
CoreSolutions-FABROCK-30_Tech Data Sheet

pdf
icon
FABROCK Stone Wool Solutions for OEM Applications - Brochure
FABROCK Stone Wool Solutions for OEM Applications - Brochure

pdf

Your recently viewed products