Compliance ASTM C612
ASTM C612

Mineral Fiber Block and Board Thermal Insulation, Type IVB Compliant

Density ASTM C303
ASTM C303

Actual Density - 12.5 lb/ft³ (200 kg/m³)

Dimensional stability ASTM C356
ASTM C356

Linear Shrinkage 1.1% @ 1200°F (650°C)

Dimensions

Contact ROCKWOOL for sizing information (1-800-265-6878)

Thickness

Contact ROCKWOOL for sizing information (1-800-265-6878)

 

Reaction to fire ASTM E84 (UL 723) - CAN/ULC S102 - CAN/ULC S114
ASTM E84 (UL 723)

Flame spread index = 0 ; Smoke development index = 0

CAN/ULC S102

Flame spread index = 0 ; Smoke development index = 0

CAN/ULC S114

Behavior of materials at 750°C (1382°F) - Non-Combustible

Thermal resistance ASTM C518 (C177)
ASTM C158 (C177)  R-value / inch @ 75ºF - 3.8 hr.ft2.F/Btu
  RSI value / 25.4 mm @ 24ºC - 0.67 m2K/W
Acoustical Performance ASTM C423
Thickness 125 Hz 250 Hz 500 Hz 1000 Hz 2000 Hz 4000 Hz NRC
1.0" 0.03 0.41 0.85 0.89 0.89 0.97 0.8
2.0" 0.39 0.73 0.81 0.86 0.97 0.95 0.85
4.0" 0.61 0.69 0.79 0.87 0.96 0.97 0.85
Reaction to moisture ASTM C1104 - ASTM C1338 - ASTM E96
ASTM C1104

Moisture Sorption by weight - <1.0%>

ASTM C1338

Determination of Fungi Resistance - Passed

ASTM E96

Water Vapor Transmission, Desiccant Method - 2360 ng/Pa.s.m2 (41 perm)

Compressive strength ASTC C165
ASTC C165

12 psi (85 kPa) @ 10% compression

ASTC C165 (@1" Thickness)

28 psi (190 kPa) @ 25% compression

Corrosion Resistance ASTM C795 - ASTM C665
ASTM C795

Stress Corrosion Cracking Tendency of Austenitic Stainless Steel - Passed

ASTM C665

Corrosion of Steel - Passed

Back
ASTM C612

Mineral Fiber Block and Board Thermal Insulation, Type IVB Compliant

Back
ASTM C303

Actual Density - 12.5 lb/ft³ (200 kg/m³)

Back
ASTM C356

Linear Shrinkage 1.1% @ 1200°F (650°C)

Back

Contact ROCKWOOL for sizing information (1-800-265-6878)

Back

Contact ROCKWOOL for sizing information (1-800-265-6878)

 

Back
ASTM E84 (UL 723)

Flame spread index = 0 ; Smoke development index = 0

CAN/ULC S102

Flame spread index = 0 ; Smoke development index = 0

CAN/ULC S114

Behavior of materials at 750°C (1382°F) - Non-Combustible

Back
ASTM C158 (C177)  R-value / inch @ 75ºF - 3.8 hr.ft2.F/Btu
  RSI value / 25.4 mm @ 24ºC - 0.67 m2K/W
Back
Thickness 125 Hz 250 Hz 500 Hz 1000 Hz 2000 Hz 4000 Hz NRC
1.0" 0.03 0.41 0.85 0.89 0.89 0.97 0.8
2.0" 0.39 0.73 0.81 0.86 0.97 0.95 0.85
4.0" 0.61 0.69 0.79 0.87 0.96 0.97 0.85
Back
ASTM C1104

Moisture Sorption by weight - <1.0%>

ASTM C1338

Determination of Fungi Resistance - Passed

ASTM E96

Water Vapor Transmission, Desiccant Method - 2360 ng/Pa.s.m2 (41 perm)

Back
ASTC C165

12 psi (85 kPa) @ 10% compression

ASTC C165 (@1" Thickness)

28 psi (190 kPa) @ 25% compression

Back
ASTM C795

Stress Corrosion Cracking Tendency of Austenitic Stainless Steel - Passed

ASTM C665

Corrosion of Steel - Passed

Back

 

 

print pdf
icon
FABROCK Stone Wool Solutions for OEM Applications - Brochure
FABROCK Stone Wool Solutions for OEM Applications - Brochure

pdf
icon
OEM Application Guide
OEM Application Guide

pdf